Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 62.0 GPa | 8990 ksi | ASTM D638 |
Quantum Composites AMC™ 2593 45% Carbon Fiber Reinforced Phenolic SMC AMC™ 2593 (126-40-139) is a carbon fiber reinforced phenolic engineered structural composite molding compound. The carbon fiber is PAN based 3K standard modulus tow. It exhibits outstanding low f.. |
|||
Tensile Modulus | 62.0 GPa | 8990 ksi | ASTM D638 |
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4197 is an epoxy high performance, 3K tow carbon fiber (PAN) reinforced engineered structural composite (ESC) molding compound designed for military and aerospace structural applications requi.. |
|||
Tensile Modulus | 62.0 GPa @Temperature 100 °C |
8990 ksi @Temperature 212 °F |
Wet; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |