Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.91 GPa | 1000 ksi | same value from ASTM and ISO test. |
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil.. |
|||
Tensile Modulus | 6.91 GPa | 1000 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp GFL14 PSU LNP* Lubricomp* GFL14 is a compound based on Polysulfone containing Glass Fiber and PTFE Lubricant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 6.91 GPa | 1000 ksi | same value from ASTM and ISO test. |
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava.. |