Mechanical Properties Metric English Comments
Tensile Modulus 3.98 GPa
577 ksi
Storage
Epoxy Technology EPO-TEK® M10-D Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..