Tensile Modulus 5.576 GPa
808.7 ksi
Storage
Epoxy Technology EPO-TEK® H20E-MP Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E-MP is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al..
Tensile Modulus 5.576 GPa
808.7 ksi
Storage
Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also ..