Polymer Property : Tensile Modulus = 5.57 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.57 GPa
808 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific)
CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla..
Tensile Modulus 5.57 GPa
808 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific)
BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance ..