Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.41 GPa | 785 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Tensile Modulus | 5.41 GPa | 785 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Tensile Modulus | 5.41 GPa | 785 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12 LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri.. |
|||
Tensile Modulus | 5.41 GPa | 785 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12 LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri.. |