Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 476 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.28 GPa
476 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 3.28 GPa
476 ksi
1 mm/min
Polimeri Europa EDISTIR N1670 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP..
Tensile Modulus 3.28 GPa
476 ksi
1 mm/min
Polimeri Europa EDISTIR N1671 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol..
Tensile Modulus 3.28 GPa
476 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK
LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.28 GPa
476 ksi
ASTM Data
Dow Tyril® 100 SAN
Data provided by Dow Chemical.
Copyright © lookpolymers.com All Rights Reserved