Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 3.28 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.28 GPa
476 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 3.28 GPa
476 ksi
1 mm/min
Polimeri Europa EDISTIR N1670 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP..
Tensile Modulus 3.28 GPa
476 ksi
1 mm/min
Polimeri Europa EDISTIR N1671 Polystyrene  (discontinued **)
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol..
Tensile Modulus 3.28 GPa
475 ksi
ASTM D638
Quantum Nylon 6/6 MoS2 Filled
Information provided by Quantum Advanced Engineering Plastics
Tensile Modulus 3.28 GPa
476 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK
LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant.
Tensile Modulus 3.28 GPa
475 ksi
ASTM D882
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin
High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Informat..
Tensile Modulus 3.28 GPa
476 ksi
ASTM Data
Dow Tyril® 100 SAN
Data provided by Dow Chemical.
Tensile Modulus 3.28 GPa
475 ksi
ASTM D-638
Axiall 2512 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Copyright © lookpolymers.com All Rights Reserved