Polymer Property : Tensile Modulus = 45000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 310 GPa
45000 ksi
PSM Industries PolyAlloys WNF-7129 Tungsten Heavy Alloy
Mil. T-21014 Class 1, SAE-AMS-T-21014 Class 1, AMS 7725 B, ASTM-B-777-87 Class 1Information Provided by PolyAlloys, a division of PSM Industries
Tensile Modulus 310 GPa
45000 ksi
Young's; DINV ENV 843-2
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an..