PSM Industries PolyAlloys WNF-7129 Tungsten Heavy Alloy

Category Metal , Nonferrous Metal , Tungsten Alloy
Manufacturer PSM Industries
Trade Name PolyAlloys
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries PolyAlloys WNF-7129 Tungsten Heavy Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mil. T-21014 Class 1, SAE-AMS-T-21014 Class 1, AMS 7725 B, ASTM-B-777-87 Class 1Information Provided by PolyAlloys, a division of PSM Industries
Physical Properties Metric English Comments
Density >= 16.85 g/cc
>= 0.6087 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 28
28
Tensile Strength, Ultimate >= 827 MPa
>= 120000 psi
Tensile Strength, Yield >= 552 MPa

@Strain 0.200 %
>= 80000 psi

@Strain 0.200 %
Elongation at Break >= 10 %
>= 10 %
1 in. gauge
Tensile Modulus 310 GPa
45000 ksi
Component Elements Properties Metric English Comments
Iron, Fe 2.9 %
2.9 %
Nickel, Ni 7.1 %
7.1 %
Tungsten, W 90 %
90 %