Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 431 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.97 GPa
431 ksi
ASTM D638
Network Polymers Kepital® F20-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Tensile Modulus 2.97 GPa
431 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Dry Blend E7130 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.97 GPa
431 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC
LNP LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing 20% Milled Glass, 10% PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.97 GPa
431 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP
SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
Tensile Modulus 2.97 GPa
431 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC
LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s).
Tensile Modulus 2.97 GPa
431 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Tensile Modulus 2.97 GPa
431 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP
LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 2.97 GPa
431 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS
EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l..
Tensile Modulus 2.97 - 3.285 GPa
431 - 476.5 ksi
UV Postcure; ASTM D638M
DSM Somos® NeXt LV Grey
The second member of the Somos® NeXt family, Somos® NeXt LV Grey delivers the durability and functionality, with a finer resolution of details and faster part processing. This third-generation, hi..
Tensile Modulus 2.97 GPa
431 ksi
ASTM D-638
Axiall 5055 Rigid PVC, Extrusion, White
Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor..
Tensile Modulus 2.97 GPa
431 ksi
ASTM D-638
Axiall 7555 Rigid PVC, Extrusion, Natural
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Tensile Modulus 2.97 GPa
431 ksi
ASTM D-638
Axiall 7555 Rigid PVC, Extrusion, White
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Tensile Modulus 2.97 GPa
431 ksi
ASTM D-638
Axiall 5055 Rigid PVC, Extrusion, Natural
Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p..
Tensile Modulus 2.97 GPa
431 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific)
LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based ..
Tensile Modulus 2.97 GPa
431 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC
LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard..
Copyright © lookpolymers.com All Rights Reserved