Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 29.66 GPa | 4302 ksi | ASTM D-638 |
PlastiComp Velocity® LCF40-PA6 High Flow Nylon 6, 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Tensile Modulus | 29.66 GPa | 4302 ksi | ASTM D638 |
PlastiComp Complet® LCF40-PA66 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |