PlastiComp Velocity® LCF40-PA6 High Flow Nylon 6, 40% Long Carbon Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Velocity®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Velocity® LCF40-PA6 High Flow Nylon 6, 40% Long Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Filler Content 40 %
40 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 290 MPa
42100 psi
ASTM D-638
Elongation at Break 1.0 %
1.0 %
ASTM D-638
Tensile Modulus 29.66 GPa
4302 ksi
ASTM D-638
Flexural Strength 428 MPa
62100 psi
ASTM D-790
Flexural Modulus 23.45 GPa
3401 ksi
ASTM D-790
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 8.54 J/cm
16.0 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
ASTM D-648