Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.92 GPa | 423 ksi | 0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638 |
Americas Styrenics STYRON™ 666LR General Purpose Polystyrene Resin
(discontinued **) STYRON™ 666LR is a medium flow general purpose polystyrene specifically designed to blend with styrene butadiene styrene block copolymers for packaging applications requiring high clarity, improved.. |