Polymer Property : Tensile Modulus = 422 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.91 GPa
422 ksi
ASTM D-638
Axiall 2500 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Modulus 2.91 GPa
422 ksi
ASTM D-638
Axiall 2501 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Modulus 2.91 GPa
422 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Molding M4910 (USP CLASS VI for TRANS 9494 only) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne