Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.753 GPa @Temperature 40.0 °C |
399.3 ksi @Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |