Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.66 GPa | 386 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | same value from ASTM and ISO test. |
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific) Mineral filled Antistatic Polycarbonate, HDT110degC type |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER F-1 weathering certified in natural color, specially designed for Pool & Spa applications. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
Tensile Modulus | 2.66 GPa @Temperature 120 °C |
386 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Tensile Modulus | 2.66 GPa | 386 ksi | same value from ASTM and ISO test. |
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |