Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 37.0 GPa | 5370 ksi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 315 g/m2 Information provided by HexCel |
|||
Tensile Modulus | 37.0 GPa | 5370 ksi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 430 g/m2 Information provided by HexCel |
|||
Tensile Modulus | 37.0 GPa @Temperature 23.0 °C |
5370 ksi @Temperature 73.4 °F |
90º, Wet; EN2561 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |
|||
Tensile Modulus | 37.0 GPa @Temperature 130 °C |
5370 ksi @Temperature 266 °F |
90º, Wet; EN2561 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |