Polymer Property : Tensile Modulus = 3670 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 25.3 GPa
3670 ksi
ISO 527-2/1A/1
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Tensile Modulus 25.3 GPa
3670 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS
LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive.
Tensile Modulus 25.3 GPa
3670 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS
LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Modulus 25.3 GPa
3670 ksi
1 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..