Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.27 GPa | 329 ksi | MD; 40 hours; 50%RH; ASTM D638 |
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave Features & Benefits:High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applicationsLow loss tangent - Excellent high frequency per.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47N ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® Z48 ABS Automotive. Very high heat resistance with medium impact and good strength properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific) Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 955AU PC (Asia Pacific) Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 925A PC Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 945U PC Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE101R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Asia Pacific) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | ISO 527-1/-2 |
BASF Ultrason® P 3010 MR SW 10101 PPSU Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 925U PC Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additi.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE101 PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). 7.0 MFR, for thicker sections without sinks.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 945 PC (Asia Pacific) Lexan* 945 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 945W PC (Asia Pacific) Lexan* 945W Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque colo.. |