Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific) High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 945A PC (Asia Pacific) Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 955AU PC Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 955AU PC (Asia Pacific) Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPM1944 PC Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPM1944 PC (Europe-Africa-Middle East) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® R9453 PC (Asia Pacific) Lexan* R9453 Polycarbonate (PC) is a non-filled, non-chlorine and non-brominate flame retardant resin for general purpose, which contains 30% post-consumer recycled PC. This resin is of UL-94 V0 rat.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 2.0 in/min; 0.125" thickness; ASTM D-638 |
Chevron Phillips MA5350 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Floppy diskettesDurable household applicationsThin to medium parts that require a combination of high gloss and good toughnessFeatures:Low coeffi.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 925A PC (Asia Pacific) Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 925U PC (Asia Pacific) Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 945U PC Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 955 PC (Asia Pacific) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE101R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp YF006 TPEE LNP THERMOCOMP* YF006 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | ASTM D638 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 925U PC Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additi.. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer 40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.27 GPa | 329 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |