Tensile Modulus 22.6 GPa
3280 ksi
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in ..
Tensile Modulus 22.6 GPa
3280 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized...
Tensile Modulus 22.6 GPa
3280 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 (Asia Pacific)
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Tensile Modulus 22.6 GPa
3280 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon DEL369E PC
LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S..
Tensile Modulus 22.6 GPa
3280 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific)
LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 22.6 GPa
3280 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66
LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive.