Polymer Property : Tensile Modulus = 32.97 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.2273 GPa

@Temperature 135 °C
32.97 ksi

@Temperature 275 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Tensile Modulus 0.2273 GPa

@Temperature 135 °C
32.97 ksi

@Temperature 275 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..