Tensile Modulus 21.86 GPa
3171 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66
LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare.
Tensile Modulus 21.86 GPa
3171 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66
LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural.