Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 21.86 GPa | 3171 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66 LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare. |
|||
Tensile Modulus | 21.86 GPa | 3171 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66 LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |