Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 30.5 GPa | 4420 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |