Mechanical Properties Metric English Comments
Tensile Modulus 3.42 GPa
496 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH1005 TPI Resin
Thermoplastic Polyimide Extem* XH1005 Resin.
Tensile Modulus 3.42 GPa
496 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1005 Resin.
Tensile Modulus 3.42 GPa
496 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1005 Resin.
Tensile Modulus 3.42 GPa
496 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East)
High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/..
Tensile Modulus 3.42 GPa
496 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH1015 TPI Resin
Thermoplastic Polyimide Extem* XH1015 Resin.
Tensile Modulus 3.42 GPa
496 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1015 Resin.
Tensile Modulus 3.42 GPa
496 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin.
Tensile Modulus 3.42 GPa
496 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH1015F TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin. EFSA food Contact approved.
Tensile Modulus 3.42 GPa
496 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear
LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant.
Tensile Modulus 3.42 GPa
496 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66
LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant.
Tensile Modulus 3.42 GPa
496 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp FF004 PE
LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.