Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.175 GPa | 460.5 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |