Mechanical Properties Metric English Comments
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Tensile Modulus 2.04 GPa
296 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® BFL4000U PC
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Tensile Modulus 2.04 GPa
296 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS
LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive.
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce..
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Tensile Modulus 2.04 GPa
296 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics GELOY CR7500 ASA
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.