Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 19.66 GPa | 2851 ksi | ASTM D638 |
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |