Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Filler Content 30 %
30 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 125
125
ASTM D785
Tensile Strength 153.8 MPa
22310 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ASTM D638
2.4 %
2.4 %
Flexural Strain; ASTM D790
Tensile Modulus 19.66 GPa
2851 ksi
ASTM D638
Flexural Strength 201 MPa
29100 psi
ASTM D790
Flexural Modulus 14.7 GPa
2130 ksi
ASTM D790
Compressive Strength 196 MPa
28400 psi
ASTM D695
Compressive Modulus 4.317 GPa
626.2 ksi
ASTM D695
Izod Impact, Notched 0.294 J/cm
0.550 ft-lb/in
ASTM D256