Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.97 GPa @Temperature -70.0 °C |
285 ksi @Temperature -94.0 °F |
50%RH; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |