Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.97 GPa | 286 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific) ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 1mm/min |
Eastman Eastalloy DA003 PC+PCTG Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | ASTM Data |
Americas Styrenics Styron® 6010 High Impact Polystyrene
(discontinued **) STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac.. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | ASTM Test |
BASF Ultraform N 2640 Z2 UNC Q600 POM Ultraform N2640 Z2 UNC Q600 is an elastomer-modified grade of POM for injection molding with high impact strength. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | ASTM D-638 |
Axiall 3020 Rigid PVC, Extrusion Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G.. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Tensile Modulus | 1.97 GPa @Temperature -70.0 °C |
285 ksi @Temperature -94.0 °F |
50%RH; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |
|||
Tensile Modulus | 1.97 GPa | 286 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR7500 ASA High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |