Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.193 GPa | 28.0 ksi | ISO 527-2/1A/1 |
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade) Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock.. |