Mechanical Properties Metric English Comments
Tensile Modulus 0.193 GPa
28.0 ksi
ISO 527-2/1A/1
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade)
Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock..