Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.922 GPa | 278.8 ksi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a.. |