Mechanical Properties Metric English Comments
Tensile Modulus 1.922 GPa
278.8 ksi
chs 2.0 in/min; ASTM D638
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade
Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a..