Mechanical Properties Metric English Comments
Tensile Modulus 18.28 GPa
2651 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON PX91060 PA 6
LNP* VERTON* PX91060 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added feature of this grade is: Structural.
Tensile Modulus 18.28 GPa
2651 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON PX91060 PA 6 (Asia Pacific)
LNP* Verton* PX91060 is a compound based on Nylon 6 resin containing Long Glass Fiber.