SABIC Innovative Plastics LNP VERTON PX91060 PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON PX91060 PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* PX91060 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added feature of this grade is: Structural.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Time 86400 sec
0.0010 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 236 MPa
34200 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Tensile Modulus 18.28 GPa
2651 ksi
50 mm/min; ASTM D638
Flexural Strength 344 MPa
49900 psi
ASTM D790
Flexural Modulus 15.3 GPa
2220 ksi
ASTM D790
Izod Impact, Notched 2.34 J/cm
4.38 ft-lb/in
ASTM D256
Izod Impact, Unnotched 13.53 J/cm
25.35 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 219 °C

@Thickness 3.20 mm
426 °F

@Thickness 0.126 in
unannealed; ASTM D648