Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.175 GPa | 25.4 ksi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.200 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Tensile Modulus | 0.175 GPa | 25.4 ksi | ISO 527/2 |
Iran Petrochemical (PCC) 1922T Low Density Polyethylene LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Co.. |
|||
Tensile Modulus | 0.175 GPa | 25.4 ksi | ISO 527-1/-2 |
DSM Arnitel® PM471 45 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.175 GPa | 25.4 ksi | ISO 527-1/-2 |
DSM Arnitel® PM471 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.175 GPa | 25.4 ksi | average; perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.130 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |