Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) 1922T Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 1922T Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ISO 1183
Environmental Stress Crack Resistance 3.0 hour
3.0 hour
DSM Method
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ISO 868
Ball Indentation Hardness 16.0 MPa
2320 psi
ISO 2039-1
Tensile Strength at Break 7.00 MPa
1020 psi
ISO 527/2
Tensile Strength, Yield 8.00 MPa
1160 psi
ISO 527/2
Elongation at Break 400 %
400 %
Tensile Modulus 0.175 GPa
25.4 ksi
ISO 527/2
Izod Impact, Notched (ISO) 42.0 kJ/m²
20.0 ft-lb/in²
ISO 180/A
Tensile Creep Modulus, 1 hour 80.0 MPa
11600 psi
ISO 899
Thermal Properties Metric English Comments
Vicat Softening Point 82.0 °C
180 °F
ISO 306
Heat Distortion Temperature 39.0 °C
102 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 105 °C
221 °F
Copyright © lookpolymers.com All Rights Reserved