Polymer Property : Tensile Modulus = 25.16 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 25.16 GPa
3649 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS
LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This ..
Tensile Modulus 25.16 GPa
3649 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED
LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.