Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2409 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 16.61 GPa
2409 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK
LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Tensile Modulus 16.61 GPa
2409 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK
LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant.