Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.45 GPa | 2386 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PH1000A PA 6 LNP THERMOCOMP* PH1000A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |