Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.86 GPa | 2300 ksi | ASTM D638 |
PlastiComp Complet® LBF50-PA66 50% Long Basalt Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Tensile Modulus | 15.9 GPa | 2300 ksi | ASTM D638 |
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer
(discontinued **) XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe.. |