Polymer Property : Tensile Modulus = 23.19 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 23.19 GPa
3363 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Faradex DX07304 PC (Asia Pacific)
CF filled grade with EMI shieldingThis data was supplied by SABIC-IP for the Asia Pacific region.