Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.152 GPa | 22.0 ksi | ASTM D638 |
3M Dyneon™ CC174-N PTFE, 15% Fiberglass/Moly Filled
(discontinued **) Product Form: Gray, non-pelletized powder. Applications include bearings, rider rings, and packings.Data provided by Dyneon. |