Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 21.3 GPa | 3090 ksi | ASTM D638 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Tensile Modulus | 21.3 GPa | 3090 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Conditioned Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |