Mechanical Properties Metric English Comments
Tensile Modulus 2.067 GPa
299.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Modulus 2.067 GPa
299.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Diamond Polymers NPP 808 C2 TDS Polycarbonate Alloy, Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.