Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 120 - 135 GPa | 17400 - 19600 ksi | |
Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfello.. |